Development Sustainable Concrete with High-volume …
The highest drop in strength with a high amount of WTCP (≥50%) was attributed to high silica concentration which directly restricted the C-(A)-S-H gels formulation and led to lower strength performance [49]. A mix with 60% WTCP met the target strength of 20 MPa at 28 days and was advanced for further experimentation.