When treating a pulp containing 10 percent solids, the respective minus 5- and minus 2-micrometer content of the ground product was 92.3 and 73.4 percent. Furthermore, the minus 5- and minus 2-micrometer content of the test at 2.5 percent solids was even lower—only 80.5 and 53.0 percent, respectively.