Grinding flotation of bituminous coal of different oxidation …
H 2 O 2 solutions of different concentrations were mixed and every 500 mL of them was added to 500 g of bituminous coal sample. The five mixtures were kept being agitated for 24 h at 20 °C.To obtain a very deeply oxidized coal, Sample 6 added with H 2 O 2 solution of 30% was agitated for 24 h at 80 °C. The detailed treatment of samples is …